This paper studies the production of lead nitrate and nitric acid reaction with galena, explore the optimal process conditions of galena wet production of lead nitrate. The results showed that: galena hydrometallurgy lead nitrate optimal condition is: reaction temperature75 C, liquid solid ratio of 3:1, the concentration of nitric acid for3N and dosage for theory volume 110%, 9 hours. The leaching reaction under this condition, the leaching rate of up to 96% lead.%用方铅矿与硝酸反应生产硝酸铅,探求方铅矿湿法生产硝酸铅最佳工艺条件。结果表明:方铅矿湿法生产硝酸铅的工艺最佳条件是:反应温度75℃,液固比3:1,硝酸浓度为3N且用量为理论量110%,9小时。浸出反应在此条件下,铅的浸出率可达96%。