Damage visualization and deformation measurement in glass laminates during projectile penetration

机译:弹丸穿透过程中玻璃层压板的损伤可视化和变形测量

获取原文
获取原文并翻译 | 示例
       

摘要

Transparent armor consists of glass-polymer laminates in most cases. The formation and propagation of damage in the different glass layers has a strong influence on the ballistic resistance of such laminates. In order to clarify the course of events during projectile penetration, an experimental technique was developed, which allows visualizing the onset and propagation of damage in each single layer of the laminate. A telecentric objective lens was used together with a microsecond video camera that allows recording 100 frames at a maximum rate of 1 MHz in a backlit photography set-up. With this technique, the damage evolution could be visualized in glass laminates consisting of four glass layers with lateral dimensions 500 mm ? 500 mm. Damage evolution was recorded during penetration of 7.62 mm AP projectiles with tungsten carbide core and a total mass of 11.1 g in the impact velocity range from 800 to 880 m/s. In order to measure the deformation of single glass plates within the laminates, a piece of reflecting tape was attached to the corresponding glass plate, and photonic Doppler velocimetry (PDV) was applied. With the photonic Doppler velocimeter, an infrared laser is used to illuminate an object to be measured and the Doppler-shifted light is superimposed to a reference light beam at the detector. The simultaneous visualization and PDV measurement of the glass deformation allow determining the deformation at the time of the onset of fracture. The analysis of the experimental data was supported by numerical simulations, using the AUTODYN commercial hydro-code.
机译:在大多数情况下,透明护套由玻璃聚合物层压板组成。不同玻璃层的损坏的形成和传播对这种层压板的抗突抗性有很大影响。为了阐明射弹穿透期间的事件过程,开发了一种实验技术,允许可视化每个单层层压板中的损坏的发作和传播。远心目标镜头与微秒摄像机一起使用,允许在背光摄影设置中以1 MHz的最大速率记录100帧。利用这种技术,可以在由四个玻璃层组成的玻璃层压板上可视化损伤进化500mm的玻璃层层。 500毫米。在7.62mm AP弹丸的渗透过程中记录损伤进化,碳化钨核心的渗透率,并且在冲击速度范围内的11.1g的总质量范围为800至880米/秒。为了测量层压板内的单玻璃板的变形,将一块反射带附着到相应的玻璃板上,并施加光子多普勒速度(PDV)。利用光子多普勒速度计,使用红外激光器照射待测物体,并且多普勒偏移光被叠加到检测器处的​​参考光束上。玻璃变形的同时可视化和PDV测量允许在裂缝开始时确定变形。使用Autodyn商业水电编码,通过数值模拟支持实验数据的分析。

著录项

  • 来源
    《兵工学报(英文版)》 |2014年第2期|226-238|共13页
  • 作者单位

    Fraunhofer Institute for High-Speed Dynamics, Ernst-Mach-Institute EMI, Am Christianswuhr 2, 79400 Kandern, Germany;

    Fraunhofer Institute for High-Speed Dynamics, Ernst-Mach-Institute EMI, Am Christianswuhr 2, 79400 Kandern, Germany;

    Fraunhofer Institute for High-Speed Dynamics, Ernst-Mach-Institute EMI, Am Christianswuhr 2, 79400 Kandern, Germany;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

  • 入库时间 2022-08-19 03:35:07
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号