Microparticle formation and crystallization rate of 1,3,5,7-tetranitro-1,3,5,7-tetraazacyclooctane (HMX) in acetone solution using supercritical carbon dioxide antisolvent (GAS) recrystallization were studied. Scanning electronic microscopy, X-ray diffraction and infrared radiation were used to examine particle size, crystallinity and chemical structure. The results show that β-HMX microparticle in different average size (2-9.5μm) and with narrow size distribution were obtained by controlling the expansibility, expansion speed, initial concentration and temperature during recrystallization of HMX. The formation of nuclei may be a main cause of consumption of solute when the solution is expanded rapidly enough and the equilibrium concentration is lower, in which almost monodisperse microparticle can be obtained.