HYPEREUTECTIC Al-Si ALLOY CASTINGS WITH A COMPLETELY EUTECTIC STRUCTURE

机译:具有全共晶结构的过共晶Al-Si合金铸件

获取原文
获取原文并翻译 | 示例

摘要

Experiments with electrolytic Al-Si alloy (DEASA) were conducted to produce the pure eutectic structure without impurity-addition in hypereutectic alloys castings at same cooling rate. Until silicon increased to 16% the coupled eutectic was achieved, accompanying a decrease in undercooling in freezing. This is associated with the inheritance of the self-modification of DEASA. With 17% Si the self-modification disappeared and the coarse primary silicon crystal occurred under undercooling of 5℃. The reason to develop the coupled eutectic structure seems to be attributed to the suppression of silicon growth in cooling range before approaching the apparent eutectic temperature by large undercooling rather than the competitive growth between two phases in eutectic.
机译:进行了电解铝硅合金(DEASA)的实验,以相同的冷却速率在过共晶合金铸件中产生了不添加杂质的纯共晶组织。直到硅含量增加到16%,才实现了共晶,伴随着冷冻中过冷度的降低。这与DEASA自我修改的继承有关。当硅含量为17%时,自我改性消失,在5℃过冷下会出现粗大的初生硅晶体。形成共晶结构的原因似乎归因于在通过大的过冷来达到表观共晶温度之前抑制冷却范围内硅的生长,而不是由于共晶两相之间的竞争性增长。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号