摘要

In this paper the technology of the poplar plywood with soy adhesive is researched. The result shows that its properties can surpass the requirement of Chinese Standard for type Ⅱ plywood. Although it is almost same to compare the technology of the soy adhesive bounded poplar plywood with the technology of the UF adhesive bounded poplar plywood, the technical parameter is difference. It is clear that the higher the temperature of hot pressing is, the better the gluing strength of the plywood is in the testing scope. The better technical parameter of the plywood is that the temperature of hot-pressing is 160℃,the time of hot-pressing is 70sec/mm (panel thickness), the pressure is 1.4 MPa, the resin content of double area is 380g/m<'2>.
机译:本文研究了含大豆胶的杨木胶合板技术。结果表明,其性能可以超过中国Ⅱ类胶合板的要求。尽管将大豆胶粘杨木胶合板的技术与UF胶粘杨木胶合板的技术进行比较几乎是相同的,但技术参数是不同的。显然,热压温度越高,胶合板在测试范围内的粘合强度越好。胶合板更好的技术参数是热压温度为160℃,热压时间为70sec / mm(面板厚度),压力为1.4MPa,双倍面积树脂含量为380g / m <'2>。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号