MCC-1 static short-term corrosion tests were performed to pyrochlore simulated waste forms in deionized water, at 90℃. Experimental results show that pyrochlore simulated waste forms has a good anti-leaching property. Both the normalized mass loss rate and the normalized mass loss of element Ce decrease with soaking time increasing in the short test. The corrosion process is co-dominated by the leaching agent and the corrosion temperature.
机译:对去离子水中的烧绿石模拟废物进行了MCC-1静态短期腐蚀试验,温度为90℃。实验结果表明,烧绿石模拟废物形态具有良好的抗浸出性能。在短时间试验中,元素Ce的归一化质量损失率和归一化质量损失都随着浸泡时间的增加而降低。腐蚀过程主要由浸出剂和腐蚀温度决定。