ACI 318-99 no longer refers to Z factors or crack width formulae as in previous editions of the code. Instead, ACI 318-99 correlates bar spacing with clear concrete cover, indicating that following these guidelines will reduce crack widths at the concrete surface. Field investigations have found leakage at certain type cracks which exhibit widths of .23mm (0.009″) or greater. Research and condition surveys completed by the author have found greater potential for concrete deterioration at cracks which extend to embedded reinforcement as compared with low slump, low water/cement ratio concrete having adequate cover over reinforcement. Current codes and standards present considerable variation with regard to recommended maximum crack widths to prevent leakage. Use of ACI 318-99 to design liquid or gas retaining structures could lead to designs that are not conservative, not durable and possibly unsafe, if preventing leakage is an important requirement for the particular facility.
机译:ACI 318-99不再像以前的版本中那样引用Z因子或裂缝宽度公式。相反,ACI 318-99将钢筋间距与清晰的混凝土覆盖层相关联,表明遵循这些准则将减小混凝土表面的裂缝宽度。现场调查发现,某些类型的裂缝的渗漏宽度为0.23毫米(0.009英寸)或更大。作者完成的研究和状况调查发现,与低坍落度,低水灰比比的混凝土具有足够的覆盖率的混凝土相比,扩展到嵌入式钢筋的裂缝处的混凝土劣化的可能性更大。当前的规范和标准在建议的最大裂纹宽度方面存在很大差异,以防止泄漏。如果防止泄漏是特定设备的重要要求,则使用ACI 318-99设计液体或气体保留结构可能会导致设计不保守,不耐用且可能不安全。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号