In the period from April to October of 1988, a series of welding operations on the outside of the AZ Tank Farmventilation line piping at the Hanford Site produced unexpected and repeated cracking of the austenitic stainless steel base metaland of a seam weld in the pipe. The ventilation line is fabricated from type 304L stainless steel pipe of 24-inch (60.96 cm)diameter and 0.25-inch (0.64 cm) wall thickness. The pipe was wrapped in polyethylene bubble wrap and buried approximately12 feet (3.66 m) below grade. Except for the time period between 1980 and 1987, impressed current cathodic protection hasbeen applied to the pipe since its installation in 1974. The paper describes the history of the cracking of the pipe, the probablecracking mechanisms, and the recommended future action for repair/replacement of the pipe.
机译:在1988年4月至10月期间,在汉福德工地的AZ Tank Farmventilation生产线管道外部进行了一系列焊接操作,导致奥氏体不锈钢基体金属出现意外和反复开裂,并在管道中产生接缝。通风管路由直径为24英寸(60.96厘米),壁厚为0.25英寸(0.64厘米)的304L型不锈钢管制成。将管道用聚乙烯气泡包装纸包裹,并埋入地下约12英尺(3.66 m)的位置。自1974年安装以来,除了1980年至1987年这段时间外,目前已对管道施加了令人印象深刻的阴极保护。本文介绍了管道破裂的历史,可能的破裂机理以及建议的维修/更换新措施。的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号