MECHANICAL CHARACTERIZATION FOR A LARGE TEST DESIGN OF A DISSIMILAR METALS WELDING WITH A NARROW GAP NICKEL ALLOY WELD: EXPERIMENTAL AND NUMERICAL ANALYSIS ON SPECIMENS

机译:具有窄间隙镍合金焊缝的不同金属焊接大型测试设计的机械表征:试样的实验性和数值分析

获取原文

摘要

Dissimilar metal welds are a common feature of light water reactors in connections between ferritic components and austenitic stainless steel piping systems. Inspection difficulties, variability of material properties and residual stresses all combine to create problems for structural integrity assessment.Within the framework of European project STYLE, a fracture test on a pipe containing a through wall crack in a narrow gap Nickel alloy Dissimilar Metals (DMWinc) is under preparation. The work is focusing on the nickel alloy - ferrite steel interface which is the weakest area of such welded pipes in front of ductile tearing. The study temperature is 300°C, which covers typical temperatures in components like hot pipes in the primary coolant system of pressurized water reactors.This paper gives an overview of the program and the first results of works which is been carried out by the French Atomic Energy Commission and Alternative Energies (CEA) in order to study the mechanical properties and integrity of component of the DMWinc pipes provided and designed by AREVA France.
机译:不同的金属焊缝是铁素体组分和奥氏体不锈钢管道系统之间的轻水反应器的共同特征。检查困难,材料性质的可变性和残余应力全部合并以创造结构完整性评估的问题。在欧洲项目风格的框架中,在狭窄的间隙镍合金不同金属(Dmwinc)中的横壁裂缝的管道上的骨折试验正在准备。该作品专注于镍合金 - 铁氧体钢接口,该钢界面是延展性撕裂前的这种焊接管的最弱区域。研究温度为300°C,涵盖了加压水反应堆的主要冷却剂系统中的热管等元件中的典型温度。本文还概述了该计划的概述和由法国原子进行的工作的第一个结果能源委员会和替代能量(CEA),以研究由Areva法国提供和设计的DMWINC管道部件的机械性能和完整性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号