Nd-YAG laser welding characteristics of Inconel 718, microstructures,tensile properties,and hardness of welding joint were researched. Nd-YAG laser welding was carried out on super thin Inconel 718 sheet(0.2 mm thick) with 6 specimens. The welding parameters of these specimens are varied expect for the welding speed(0.3mm/s), gas-flow rate (5L/min) and clearance between focal point and (plate) surface(0).In this research,the tensile strength of welding joint was found to be inferior to base metal and the ductility of welds was considerably lower than base material,the microhardness in weld zone is higher than the base material hardness and the hardness is highest in center zone of welding joint. These conclusions will be in favour of the manufacture with super thin Inconel 718.
机译:研究了Inconel 718,微观结构,拉伸性能和焊接接头硬度的Nd-YAG激光焊接特性。 ND-YAG激光焊接在具有6个标本的超薄Inconel 718片(0.2mm厚)上进行。 这些样品的焊接参数随着焊接速度(0.3mm / s),气流速率(5L / min)和焦点和(板)表面之间的间隙而变化,焊接速度(0)。在本研究中,拉伸强度 焊接接头被发现较差,焊缝的延展性明显低于基材,焊接区的显微硬度高于基材硬度,硬度在焊接接头的中心区域中最高。 这些结论将有利于用超薄的薄膜718制造。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号