Sewage sludge might result in secondary pollution if there were unreasonable disposal methods. The traditional methods of disposing sludge included incineration, land use, reclamation, etc. If the sludge mixed with shale was fired to make haydite, the problem could be solved; in addition, it could produce high-performance artificial ultra-lightweight aggregate. Dehydrated sludge and shale was chosen to produce ultra-lightweight haydite by analysis of chemical and mineral composition for raw materials and considering haydite production processes and raw materials requirements. It had high strength and low water absorption at certain technical conditions. Optimal mixing ratio and baking system is obtained as follows: sludge dosage of 30%, preheating temperature of 400°C, preheating time of 10 min, baking temperature of 1150°C, baking time of 12 min. Haydite performances show: apparent density of 508 kg/m3, density level of 300, 1 hour water absorption of 6.0%, particle strength of 200N.
机译:如果有不合理的处置方法,污水污泥可能会导致二次污染。传统的处理污泥的方法包括焚烧,土地使用,填海层等如果将污泥与页岩混合射击制作哈迪特,则可能会解决问题;此外,它还可以生产高性能人工超轻量级骨料。选择脱水污泥和页岩,通过分析原料的化学和矿物组合物,并考虑干草生产工艺和原料要求,通过分析化学和矿物组合物来生产超轻量级的雨披。它在某些技术条件下具有高强度和低吸水性。获得优化的混合比和烘焙系统如下:污泥剂量为30%,预热温度为400° c,预热时间10分钟,烘烤温度为1150° c,烘烤时间12分钟。 Haydite表演表明:表观密度为508 kg / m 3 ,密度水平为300,1小时吸水量为6.0%,粒度为200n。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号