首页> 外文会议>International Seminar on Metallurgy and Materials >Extraction of Magnesium from Calcined Dolomite Ore Using Hydrochloric Acid Leaching
【24h】

Extraction of Magnesium from Calcined Dolomite Ore Using Hydrochloric Acid Leaching

机译:盐酸浸出煅烧白云岩矿石镁的提取

获取原文

摘要

Magnesium is widely used in varieties industrial sector. Dolomite is one source of magnesium besides seawater. The extraction of magnesium from dolomite ores can be done by leaching process. In this work, the dolomite leaching to extract magnesium by hydrochloric acid was investigated. The leaching experiments were performed in a spherical glass batch reactor having a capacity of 1000 ml. The effects of the stirring speed, acid concentration, reaction temperature and liquid-solid ratio for each reaction time of 1; 2; and 3 h on the Mg leaching have been evaluated. 5 ml of solution sample were collected from the leached solutions, then it was filtered prior to analysis by ICP OES. The experimental results show that the magnesium extraction increases along with the increase of acid concentration, liquid-solid ratio and temperature. The optimum conditions for magnesium extraction were achieved at temperature 75 °C, extraction time 3 h, the HC1 concentration of 2 M, the liquid-solid ratio 20 ml/g and stirring speed of 400 rpm. At this condition 98,82 % of magnesium were extracted from dolomite. The conclusion obtained from this leaching process is that the magnesium can be extracted from dolomite by using hydrochloric acid solutions.
机译:镁广泛用于品种工业部门。除海水之外,白云石是镁的一个来源。从白云石矿石中镁的提取可以通过浸出过程来完成。在这项工作中,研究了通过盐酸提取镁的白云石浸出。浸出实验在球形玻璃批量反应器中进行,其容量为1000mL。每次反应时间为1的搅拌速度,酸浓度,反应温度和液态比的影响; 2;已经评估了3小时的Mg浸出。从浸出的溶液中收集5ml溶液样品,然后通过ICP OES分析之前过滤。实验结果表明,镁萃取随着酸浓度,液态比和温度的增加而增加。在温度75℃下实现最佳条件,提取时间3小时,HC1浓度为2μm,液体 - 固体比20ml / g和400rpm的搅拌速度。在这种情况下,从白云石中提取98,82%的镁。从该浸出过程中获得的结论是通过使用盐酸溶液,可以从白云石中萃取镁。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号