The focus of this work has been microstructure characterisation of Ti-6Al-4V manufactured by five different additive manufacturing (AM) processes. The microstructure features being characterised are the prior (3 size, grain boundary a and a lath thickness. It was found that material manufactured with powder bed fusion processes has smaller prior β grains than the material from directed energy deposition processes. The AM processes with fast cooling rate render in thinner a laths and also thinner, and in some cases discontinuous, grain boundary a. Furthermore, it has been observed that material manufactured with the directed energy deposition processes has parallel bands, except for one condition when the parameters were changed, while the powder bed fusion processes do not have any parallel bands.
机译:该工作的重点是由五种不同添加剂制造(AM)工艺制造的Ti-6Al-4V的微观结构表征。 所表征的微观结构特征是先前的(3尺寸,晶界A和板条厚度。发现用粉末床融合过程制造的材料比来自定向能量沉积工艺的材料更小的β颗粒。AM流程快速 冷却速度呈较薄的板条和也更薄,并且在某些情况下不连续,晶界A。此外,已经观察到与定向能量沉积过程制造的材料具有平行带,除了改变参数时的一个条件, 虽然粉末床融合过程没有任何平行带。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号