The generation of mining waste has been the subject of environmental, economic and social concern. Alternative and sustainable methods of recycling metals technologies are desired. The present work focuses on the application of the ion exchange technique for the extraction of metals contained in a lateritic nickel mining effluent. The Purolite S950 chelating resin was used in the present work because it has the ability to adsorb transition metals present in an acidic solution. The experiments were carried out in a batch varying the pH in the range of 0.5-2.0. 1 g of resin was placed in contact with 50 mL of solution and stirred for 120 min at a speed of 200 rpm and temperature at 25°C. The results demonstrated that the affinity of the resin varied with pH. The adsorbed metals were only copper, manganese, magnesium and zinc. The most extracted metal was copper, corresponding to 37%, when the solution was conditioned at pH 2.0.
机译:采矿废物的产生是环境,经济和社会问题的主题。期望再循环金属技术的替代和可持续的方法。本作本作侧重于离子交换技术的应用,以萃取外侧镍采矿流出物中所含的金属。在本作工作中使用猪岩S950螯合树脂,因为它具有吸附在酸性溶液中存在的过渡金属的能力。实验在0.5-2.0的水批量中,在批量中进行。将1g树脂与50ml溶液接触,并以200rpm的速度和25℃的温度搅拌120分钟。结果表明,树脂的亲和力随pH而变化。吸附的金属仅是铜,锰,镁和锌。当溶液在pH2.0下将溶液调节时,最萃取的金属是铜,对应于37%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号