Preservation of Archaeological Leather by Reinforcement with Styrene Butadiene Rubber

机译:用苯乙烯丁二烯橡胶加固防治考古皮革

获取原文

摘要

Leather has been used in Egypt since 4000 BC. Ancient Egyptians used leather as shrouds, bookbinding and manuscripts. This research aims to find a way to protect archeological leather from damage by environmental factors, without losing their archaeological appearance. Leather samples were subjected to ageing in order to simulate archaeological leather. Styrene butadiene rubber was used to coat the leather samples. Then the leather samples were dipped (immersed) in a bath containing SBR dissolved in toluene with concentrations varies from 1 to 5% by weight. The effect of leather/ SBR reinforcement was evaluated by Fourier Transform Infrared Spectrometry (FTIR) and measuring the mechanical properties (tensile strength and elongation at break (%), color difference (AE) and lightness (L), pH value before and after ageing. In addition, Scanning Electron Microscope (SEM) was used to study the surface morphology of samples. Finally, all samples were subjected to ageing after reinforcement. The results revealed that reinforcement of leather samples by SBR solutions having concentration 3 % gave the best results among other concentrations. The mechanical properties of treated samples were enhanced with reduction in the AE values. The results also showed that the pH values of the treated samples did not change even after further aging. SEM scans evidenced that SBR filled the leather surface cracks besides the formation of a protective layer on the leather surface.
机译:自4000年以来,皮革已在埃及使用。古埃及人用皮革作为裹尸布,装订和手稿。该研究旨在找到一种方法来保护考古皮革免受环境因素损坏的方法,而不会失去考古外观。为了模拟考古皮革,对皮革样品进行老化。苯乙烯丁二烯橡胶用于涂层皮革样品。然后将皮革样品浸渍(浸入含有SBR的浴中,浓度从1-5重量%变化。通过傅里叶变换红外光谱法(FTIR)评估皮革/ SBR加固的效果,测量机械性能(抗拉强度和断裂(%),色差(AE)和亮度(L),在老化之前和之后的pH值。另外,扫描电子显微镜(SEM)用于研究样品的表面形态。最后,所有样品均在增强后进行老化。结果表明,通过浓度的SBR溶液加固3%的皮革样品得到了最佳结果在其他浓度之外。通过降低AE值来增强处理样品的机械性能。结果还表明,即使在进一步老化之后,处理的样品的pH值也没有改变。SEM扫描除了SBR填充皮革表面裂缝在皮革表面上形成保护层。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号