A hydroxamate collector AM28 is used in conjunction with Potassium Amyl Xanthate (PAX) to allow the flotation of the low-grade copper oxide ores from DongChuan Mine. A series of batch laboratory scale flotation tests are conducted for oxide copper minerals to establish the flotation response and the suitability of the collectors. From the rougher flotation tests performed, the highest copper recovery obtained is 78.9% at a concentrate grade of 2.5% using AM28 dosage of 740g/t and PAX dosage of 20g/t. With one stage of cleaning, the obtained copper grade increases to 9.6% with the copper recovery at 64.9%.
机译:将羟肟酸酯收集器AM28与氨基黄嘌呤(PAX)结合使用,以允许来自DongChuan Mine的低级铜氧化物矿石的浮选。 一系列批量实验室浮标测试用于氧化铜矿物,以建立浮选响应和收集器的适用性。 从令人讨厌的浮选试验中,使用的浓度为740g / t的浓缩剂等级为2.5%而获得的最高铜回收率为2.5%,并为20g / t的PAX剂量为78.9%。 通过一个清洁阶段,所获得的铜级增加到9.6%,铜回收率为64.9%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号