One binuclear mono-cyclopentadinyl titanocene, CpTiCl_3(CH_2)_4CpTiCl_3, has been synthesized by a new ways and characterized by (~1)H-NMR spectroscopy and elemental analysis. Its aqueous medium polymerization properties of methyl methacrylate (MMA) have been pursued with an anionic surfactant, sodiumn dodecylsulfate (SDS) in water. The obtained polymers were characterized by gel permeation chromatography (GPC). GPC results showed that the dinuclear titanium complex might provide PMMA with broad PDI (PDI=10.82). Influences of reaction parameters, such as temperature, time, MMA/Cat (molar ratio) and water amount were studied in detail. Under the conditions of the temperature was 55°C, the reaction lasted 15h, the molar ratio of Cat to MMA was 1:200, and the volume of water consumed was 40 ml, the conversion of MMA was as high as 70%.
机译:一种双核单环戊二烯基二烯烃,CPTICL_3(CH_2)_4CPTICL_3已通过新的方式合成,并以(〜1)H-NMR光谱和元素分析为特征。它的甲基丙烯酸甲酯(MMA)的水性培养基聚合性能已经用阴离子表面活性剂,SODIUMN十二烷基硫酸盐(SDS)在水中追踪。通过凝胶渗透色谱法(GPC)表征获得的聚合物。 GPC结果表明,二核钛络合物可以提供具有宽PDI的PMMA(PDI = 10.82)。详细研究了反应参数,例如温度,时间,MMA /猫(摩尔比)和水量的影响。在温度的条件下为55℃,反应持续15小时,猫至MMA的摩尔比为1:200,所用水量为40毫升,MMA的转化率高达70%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号