Fe/La-HMS was in situ techniques synthesized by using sol-gel method at room temperature, and was characterized by XRD, SEM, H_2-TPR and N_2 adsorption measurements. Without any organic solvent, the catalyst was used in selective oxidation of benzyl alcohol with 30% aqueous hydrogen dioxide as the oxidant, and the effects of the amount of metal doping, reaction time, reaction temperature, catalyst dosage and dosage of oxidant on the oxidation of benzyl alcohol were examined. The results show that partial Fe~(3+) and La~(3+) ions were incorporated into the framework of HMS partially, and Fe/La-HMS had a uniform mesoporous structure. And at 80°C, when n(H_2O_2)/n(benzyl alcohol)=2:l, n(Fe)/n(La)=10:1, catalyst dosage 3% and reaction time 4 h, the conversion of benzyl alcohol and the selectivity of benzyl aldehyde reached 63.8% and 92.2%. At the same time, catalytic activity does not change after using three times.
机译:Fe / La-HMS是通过在室温下使用溶胶 - 凝胶法合成的原位技术,其特征在于XRD,SEM,H_2-TPR和N_2吸附测量。没有任何有机溶剂,催化剂用于苄醇的选择性氧化,其二氧化氢水为氧化剂,以及金属掺杂量,反应时间,反应温度,催化剂剂量和氧化剂的用量的效应检查苄醇。结果表明,部分Fe〜(3+)和La〜(3+)离子部分掺入部分HMS的骨架中,Fe / La-HMS具有均匀的介孔结构。在80℃下,当N(H_2O_2)/ N(苄醇)= 2:1,N(Fe)/ N(La)= 10:1,催化剂剂量3%和反应时间4小时,转化苄基醇和苄基醛的选择性达到63.8%和92.2%。同时,使用三次后催化活性不会改变。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号