首页> 外文会议>Asia-Pacific Internatinal Symposium on Aerospace Technology >Mechanical Property of Friction Stir Welded Butt Joint in 2 mm Thick Aluminum Alloy
【24h】

Mechanical Property of Friction Stir Welded Butt Joint in 2 mm Thick Aluminum Alloy

机译:2 mm厚铝合金摩擦搅拌焊接对接接头的力学性能

获取原文

摘要

Two sizes of welding tool are used to prepare friction stir welded butt joint of 2024-T3 Aluminum alloy of 2mm thickness and their mechanical properties are evaluated. Indentation hardness tests revealed that typical hardness reduction is not necessarily observed on the section of the welding line. This result is different from that for thicker FSW plate. Static tests result indicates the yield stress for FSW joint is equal or a little higher than that for base material, while its ultimate strength is a little lower than that for base material. Fatigue test result indicates the several types of fatigue fracture origin such as LOP, burr, tool mark and etc are observed. Because the LOP, the tool mark and the burr exists along the welding line, these might cause multiple fracture origin and it might decrease the fatigue life significantly. Although the size of weld tool affected the size of the tool mark and the burr of the FSW, even smaller burr could be the fracture origin and affected the fatigue life.
机译:两种尺寸的焊接工具用于制备2024-T3铝合金的摩擦摩擦焊接接头,厚度为2mm厚度,并评估其机械性能。压痕硬度测试显示,在焊接线的截面上不一定观察到典型的硬度降低。该结果与较厚的FSW板不同。静态试验结果表明FSW接头的屈服应力等于或高于基材的屈服应力,而其极限强度比基材的最终强度略低。疲劳试验结果表明,观察到诸如LOP,BURR,刀具标记等的几种类型的疲劳裂缝起源。由于圆船,刀具标记和毛刺沿焊接线存在,因此可能导致多个骨折起源,因此可能会显着降低疲劳寿命。虽然焊接工具的尺寸影响了刀具标记的大小和FSW的毛刺,但甚至更小的毛刺可能是骨折起源并影响疲劳寿命。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号