The corrosion resistance of copper-nickel 90/10 and 70/30 tubes for heat exchangers was evaluated in 0.5 ppm-chlorinated seawater,under controlled service conditions in a bespoke test loop.The results were compared to Al-Brass tubes tested under the same conditions.Copper-Nickel 90/10 tubes were tested with two different geometries: internal smooth surface and internal finned surface(helix geometry).Internal pitting corrosion resistance was evaluated under simulated heat transfer conditions at two controlled skin temperatures from the internal and the external parts of the tubes for 6 months,at SOC(Tskin-in/35tC(iseawater)and 70”C(Tskin-in)/35
机译:在定制试验回路中的受控服务条件下,在0.5ppm氯化海水中评价铜镍90/10和70/30管的耐腐蚀性。结果与在相同下测试的Al-Brass管比较的结果条件。用两种不同的几何形状测试了氯镍90/10管:内部光滑表面和内部翅片表面(螺旋几何)。在来自内部和外部的两个受控皮肤温度下的模拟传热条件下评价了内部蚀腐蚀性。零件的管6个月,在SoC(Tskin-In / 35TC(IseaWater)和70“C(Tskin-In)/ 35

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号