Failure Analysis on Fracture of 16Mn Steel

机译:16Mn钢骨破裂失效分析

获取原文

摘要

Based on a system of macro & micro fracture appearance observation, energy spectrum analysis, metallurgical structure inspection and hardness test, the fracture mechanism and cause of specimen of 16Mn steel were obtained. The results showed that the large load was the main reason for the 16Mn steel specimen fracture, the fracture surfaces were different dimensional equiaxed dimples and some spherical particles which contain higher Mn, Si and O. The spherical particles may be an oxide which may be caused by the manufacturing process.
机译:基于宏观和微骨折外观观察系统,能量谱分析,冶金结构检测和硬度试验,获得16Mn钢标本的断裂机理和原因。 结果表明,大载荷是16Mn钢试样骨折的主要原因,裂缝表面是不同的尺寸等式凹槽和含有较高Mn,Si和O的球形颗粒。球形颗粒可以是可能引起的氧化物 通过制造过程。