Poly(lactic acid) films were prepared by melt-extrusion and then drawn at 90°C. These samples were soaked in acetone for 1 min. The films in acetone became cloud by the crystallization and the generation of void. The crystalliniity of the soaked drawn film was as same as that of the soaked undrawn film. The melting point of the soaked film unexpectedly decreased with the increase of draw ratio. The crystallization mechanism by heat is different from that by solvent.
机译:通过熔融挤出制备聚(乳酸)膜,然后在90℃下拉伸。将这些样品浸泡在丙酮中1分钟。丙酮中的薄膜通过结晶和空隙产生而变成云。浸泡的薄膜的结晶与浸泡薄膜的结晶相同。随着拉伸比率的增加,浸泡膜的熔点意外降低。通过热量的结晶机理与溶剂不同。