In this article a new process of using ammonia and ammonium chloride solution to leach zinc calcine and electrowinning high-purity zinc has been developed successfully. The average leaching ratio of zinc was about 93%. The impurities, such as Cu, Cd and Pb, in the filtrate were cemented completely by using zinc powder with two-stage countercurrent. At different current density, the current efficiency is higher than 93.8%. During electrowinning cell voltage is about 3.0 volt and power consumption ranges from 2550 to 2650kWh/t zinc. The zinc content in the electrowinned zinc is more than 99.999%, and the contents of the impurities of Cu, Cd, Co, Ni, Fe, As and Sb are lower than 0.0001% respectively, and lead is lower than 0.0003%.
机译:在本文中,成功地开发了使用氨和氯化铵溶液与浸出锌氧化锌和电氢化高纯度锌的新方法。锌的平均浸出率约为93%。通过使用具有两级逆流的锌粉完全巩固滤液中的杂质,例如Cu,Cd和Pb。在不同的电流密度下,电流效率高于93.8%。在电灌进期间,电池电压约为3.0伏,功耗范围为2550至2650kWh / T锌。电绕组锌中的锌含量大于99.999%,Cu,Cd,Co,Ni,Fe,AS和Sb的杂质的含量分别低于0.0001%,铅低于0.0003%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号