PRECIPITATION HARDENING S.S. CENTRIFUGAL COMPRESSOR IMPELLERS FAILURE - A CASE HISTORY - LABORATORY STUDIES -REMEDIAL ACTIONS

机译:沉淀硬化S.S.离心式压缩机叶轮失败 - 一种案例历史 - 实验室研究 - 一种方法

获取原文

摘要

17-4 PH, Precipitation Hardening Stainless Steel (ASTM A 705 Grade 630), is widely employed in several industrial fields because of its favourable combination of excellent mechanical properties and good corrosion resistance. An important application of 17-4 PH is the construction of centrifugal compressor impellers, where performance benefits from the steel's high mechanical resistance even when it is necessary to limit hardness to 33 HRC (as per NACE MR0175) to avoid devastating sulfide stress cracking phenomena (for example in sour environments). Nevertheless, there has been a case in which impellers made of 17-4 PH (hardness less than 33 HRC) have been subject to failures. It was a centrifugal compressor employed in a gas lifting service in which the fluid entrained water with a high level of salinity. Laboratory failure analysis attributed the damage to chloride stress corrosion cracking phenomena and was followed by a study on the behaviour of 17-4 PH in chloride-rich environments and on the action to take to avoid damage causing forced outages and loss of production.
机译:17-4 pH,沉淀硬化不锈钢(ASTM A 705级),由于其优异的机械性能和良好的耐腐蚀性,因此在多个工业领域被广泛使用。 17-4 pH的重要应用是对离心式压缩机叶轮的构造,其中,即使有必要将硬度限制在33小时(根据NACE MR0175)以避免破坏硫化硫化物应力裂解现象(例如在酸环境中)。然而,有一种情况,其中由17-4 pH(硬度小于33 HRC)的叶轮已经受到故障。它是一种用于气体提升服务的离心式压缩机,其中流体夹带的水分高盐度。实验室失效分析归因于氯化物应力腐蚀裂解现象的损害,然后研究了富含氯化物的环境中17-4 pH的行为以及采取行动的研究,以避免损坏导致强迫中断和生产损失。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号