EFFECT OF POSTWELD HEAT TREATMENT CONDITIONS ON MICROSTRUCTURE OF 9CR-1MO-V STEEL WELDS FOR PRESSURE VESSEL

机译:焊热处理条件对压力容器9Cr-1Mo-V钢焊缝微观结构的影响

获取原文

摘要

We investigated the effects of post-weld heat treatment conditions on the microstructure of the multi-pass submerged arc weld metal of 9Cr-1Mo-V steel used in pressure vessels. The microstructural properties were analyzed under three conditions (as-weld, Larson-Miller parameter (LMP) = 21.38 × 10~3, and LMP = 21.99 × 10~3). The precipitation behavior was observed using scanning electron microscopy, and the difference in precipitation behavior in the "as-welded" and "reheated" regions of the prepared multi-pass weld metal was clarified at the different LMP values. The precipitate was analyzed using scanning transmission electron microscopy. An oxide and two types of precipitates were identified, and a dislocation network pinned by MX-type carbides was visualized under the low-LMP condition. The effects of LMP on the effective grain size and dislocation amount were also evaluated using electron back-scattering diffraction. All microstructural change along the LMP had a positive effect on the toughness of weld metal.
机译:我们研究了在多遍埋弧焊焊在压力容器中使用的9Cr-1Mo钢-V钢的金属的显微组织的焊后热处理条件的影响。三种条件下的微结构性质进行分析(如焊缝,拉森 - 米勒参数(LMP)= 21.38×10 -3,和LMP = 21.99×10 -3)。使用扫描电子显微镜观察到的沉淀行为,并在“作为焊接”和“再加热”所准备的多遍焊接金属的区域中析出行为的差异在不同LMP值被澄清。利用扫描透射电子显微镜将沉淀物进行分析。的氧化物和鉴定两种类型的沉淀物,并通过MX型碳化物钉扎的位错网络是在低LMP的条件下可视化。 LMP对有效晶粒直径和错位量的影响进行了使用电子背散射衍射还评价。沿着LMP所有微观结构变化对焊缝金属的韧性具有积极效果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号