ALLOWABLE FLAW SIZE OF JAPANESE CAST STAINLESS STEEL PIPE USING PROBABILISTIC FRACTURE MECHANICS METHOD

机译:使用概率骨折力学方法,允许日本铸造不锈钢管的允许缺陷尺寸

获取原文

摘要

The cast austenitic stainless steel (CASS) that is used for the primary loop pipes of nuclear power plants is susceptible to thermal ageing during plant operation. The Japanese JSME rules on fitness-for-service (JSME rules on FFS) for nuclear power plants specify the allowable flaw depths. However, some of these allowable flaw sizes are small compared with the smallest flaw sizes, which can be detected by nondestructive testing. ASME Section XI Code Case N-838 recently specified the maximum tolerable flaw depths for CASS pipes determined by probabilistic fracture mechanics (PFM). In a similar way, the allowable flaw depths of CASS pipes were calculated by PFM analysis code "PREFACE" which considers uncertainty of the mechanical properties of Japanese PWR CASS materials. In order to confirm the validity of PREFACE, the allowable flaw depths calculated by PREFACE were compared with the maximum tolerable flaw depths in the technical basis of Code Case N-838. As a result, although the J calculation method and the embrittlement prediction model of CASS are different, these were qualitatively consistent. In addition, the sensitivity of ferrite content to the allowable flaw depths was investigated.
机译:用于核电厂主要环管管的铸造奥氏体不锈钢(CASS)易于在植物操作期间热老化。核电厂的健身服务的日本JSME规则(关于FFS上的JSME规则)指定了允许的漏洞深度。然而,与最小缺陷尺寸相比,这些允许缺陷尺寸中的一些较小,这可以通过非破坏性测试来检测。 ASME部分XI码案例N-838最近指定了由概率骨折力学(PFM)确定的CASS管的最大可容忍漏洞深度。以类似的方式,通过PFM分析码“前言”计算CASS管的允许漏洞深度,其考虑日本PWR CASS材料的机械性能的不确定度。为了确认前言的有效性,通过代码案例N-838的技术基础将通过前言计算的允许漏洞深度进行比较。结果,尽管CASS的j计算方法和CASS的脆化预测模型是不同的,但这些是定性一致的。此外,研究了铁氧体含量对允许漏洞深度的敏感性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号