PHASE FORMATION STUDIES USING X-RAY DIFFRACTION AND INFRARED SPECTROSCOPY IN THE VITRIFICATION OF SAVANNAH RIVER SITE SB4 HLW SLUDGE SURROGATE WITH HIGH IRON AND ALUMINUM CONTENTS AT HIGH WASTE LOADINGS

机译:使用X射线衍射和红外光谱法在大草原河段SB4 HLW污泥玻璃中使用高钢铁和铝含量高废料载体的相形成研究

获取原文

摘要

Phase formation mechanisms associated with the vitrification of Savannah River Site (SRS) Sludge Batch 4 (SB4) high level waste surrogate with high iron and aluminum contents were studied by X-ray diffraction (XRD) and infrared spectroscopy (IRS). Two mixtures at 60 and 70 wt% SB4 waste loading were prepared as slurries with a water content of ~50 wt% using a waste surrogate and commercially available Frit 503-R4 (Li_3O - 8 wt %, B_2O_3 - 16 wt %, SiO_2 - 76 wt %). The mixtures were air-dried at a temperature of 115 °C and heat-treated at 500, 700, 900, 1000, 1100, 1200, and 1300 °C for 1 hr at each temperature. IR spectra and XRD patterns of the products heat-treated at each temperature were recorded. In both the mixtures phase formation reactions started at low temperatures and yielded intermediate phases (sodalite, pyroxene-type, nepheline), and reactions were mostly completed within the temperature range between 1000 and 1100 °C. The glassy materials prepared at 1200 °C were composed of vitreous phase and magnetite/trevorite type spinel. The materials with 60 wt.% waste loading prepared at 1300 and 1400 °C had the same phase composition whereas at 70 wt.% waste loading, nepheline phase was also detected resulting from crystallization from the melt.
机译:通过X射线衍射(XRD)和红外光谱(IRS)研究了与高铁和铝含量的高钢和铝含量的玻璃化相关的相位形成机制。使用废物替代品和可商购的玻璃料(Li_3O - 8wt%,B_2O_3 - 16wt%,SiO_2)制备了在60和70wt%的Sb4废物含量为含水含量为〜50wt%的浆料。 76wt%)。将混合物在115℃的温度下在115℃的温度下在500,700,900,000,1100,1200和1300℃下在每个温度下进行热处理1小时。记录在每个温度下热处理产品的IR光谱和XRD图案。在两种混合物中,在低温下开始,在低温下开始并得到中间相(钠钠,冰石型,尼触线),并且在1000至1100℃之间的温度范围内完成反应。在1200℃下制备的玻璃状物质由玻璃体相和磁铁矿/三晶型尖晶石组成。具有60重量%的材料。在1300和1400℃下制备的%废物负载具有相同的相组合物,而在70重量%中具有相同的相组合物,也可以检测到从熔体中结晶产生肾内相。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号