【24h】

Thermodynamic Analysis for Formation of Ti(C,N) in Blast Furnace and Factors Affecting TiO_2 Activity

机译:高炉中Ti(C,N)形成的热力学分析及影响TiO_2活性的因素

获取原文

摘要

The effect of protecting blast furnace (BF) can be achieved by smelting the iron ores containing titanium. The formation of Ti(C,N) in the slag causes bubbles resulted in the difficult separation of slag and iron. The concentration of titanium in hot metal with slag-iron reaction reaching equilibrium and the solubility of titanium in hot metal are calculated by FactSage software. The results show that the concentration of titanium in hot metal with slag-iron reaction reaching equilibrium is equal to 1.042% and the solubility of titanium in hot metal is 0.5588. The most effective factor of decreasing TiO_2 activity is binary basicity (R_2=CaO/SiO_2), followed by temperature, MgO content, Al_2O_3 content.
机译:保护高炉(BF)的效果可以通过熔炼含有钛的铁矿石来实现。在炉渣中形成Ti(C,N)导致气泡导致炉渣和铁的难度分离。通过Factsage软件计算具有达到平衡的热金属中的热金属中的钛的浓度和钛的钛的溶解度。结果表明,具有刚渣 - 铁反应的热金属中钛的浓度等于1.042%,热金属中钛的溶解度为0.5588。减少TiO_2活性的最有效因素是二进制碱基(R_2 = CaO / SiO_2),然后是温度,MgO含量,AL_2O_3内容。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号