Dynamic Collapse Test of Cracked Pipes

机译:裂纹管的动态折叠试验

获取原文

摘要

In order to clarify the behavior of cracked pipes under seismic events, cyclic four point bending tests were conducted on the staight pipes with flaws. In the tests, real stress corrosion cracks (SCC) and artificial electric discharge machining (EDM) motches were induced on pipes as flaws. The specimens were subjected to the constant amplitude loading wave or the random amplitude wave. In comparison with the natural crack as SCC and the artificial crack as EDM notch, the EDM notch was easier to cause the leak of water than SCC. For the estimation of the failure on the cracked pipes. Net Section Collapse Failure Criterion (NSCFC) has been proposed and widely used under the monotonic loading conditions. To extend the thought of NSCFC to the cyclic loading condition, the method using NSCFC and fatigue life prediction was found to be useful.
机译:为了澄清地震事件下破裂管道的行为,循环四点弯曲试验是在缺陷的方形管道上进行的。在测试中,真正的应力腐蚀裂缝(SCC)和人造电气放电加工(EDM)MOTCHES在管道上被诱导诱导。将标本进行恒定幅度负载波或随机幅度波。与SCC的自然裂缝和人工裂缝相比,作为EDM缺口,EDM缺口更容易导致水泄漏而不是SCC。估计破裂管子上的故障。在单调负载条件下提出并广泛使用了净段折叠失效标准(NSCFC)。为了将NSCFC的思想扩展到循环负载条件,发现使用NSCFC和疲劳寿命预测的方法是有用的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号