The nickel-cobalt sulphides produced from limonitic laterite ores by Moa Nickel S.A. in Cuba are shipped to the Corefco nickel-cobalt refinery in Canada. This refinery is the former Sherritt Gordon nickel refinery in Fort Saskatchewan, Alberta, which has been in operation since 1954. Major changes to the refining process were required to handle the Moa sulphide feed with its unusually high cobalt content. While the ammonia leach and hydrogen reduction circuits were retained with only minor modifications, major changes were made in the processes for the separation and recovery of cobalt. A totally new cobaltnickel separation was successfully developed, in which most of the cobalt is separated from the ammoniacal nickel sulphate leach solution by precipitation as a cobalt-nickel hexammine salt, using anhydrous ammonia as the reagent. This salt, which contains equal amounts of cobalt and nickel, is refined to a pure cobaltic hexammine salt by selectively leaching nickel with water, and recrystallizing the resulting impure cobaltic hexammine salt in ammonium sulphate solution. The recrystallized cobalt hexammine salt has a Co : Ni ratio of over 2000 : 1, and contains very low levels of copper, zinc and cadmium. It is redissolved in ammonium sulphate solution and coverted to cobalt powder by hydrogen reduction. This paper describes the changes made to the refinery processes since 1991, and reviews recent operating performance with emphasis on the treatment of Moa sulphides.
机译:由MoA镍S.A.由MoA镍S.A的镍钴硫化物由MoA镍S.A.在加拿大的Corefco镍钴炼油中运送。这家炼油厂是萨斯喀彻温省艾伯塔省萨斯喀彻温堡的前谢特戈登镍炼油厂,自1954年以来一直在运作。需要用异常高钴含量处理炼油过程的重大变化来处理MOA硫化物饲料。虽然氨浸出和氢气还原电路仅存在微小的修饰中,但在钴的分离和恢复过程中进行了重大变化。成功地开发了全新的钴硝基克利分离,其中大部分钴通过作为试剂的无水氨水作为钴 - 镍己氨基己酰胺与氨基硫酸镍浸出溶液分离。该盐,其含有等量的钴和镍,通过用水选择性地浸出纯钴己氨基盐,并在硫酸铵溶液中重结晶所得的不纯的钴己酰胺盐。重结晶钴己氨盐具有2000多个:1的CO:Ni比例,含有非常低水平的铜,锌和镉。将其重新溶解在硫酸铵溶液中,并通过氢气覆盖至钴粉末。本文介绍了自1991年以来对炼油过程的变化,并评论了最近的经营性能,重点是对MoA硫化物的治疗。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号