Laboratory and pilot scale testing were carried out in 1999 on a tailing sample from a North American iron ore plant using gravity, magnetic and flotation techniques. The ore contained 16 per cent iron mainly in the fine (–38 μm) size fraction. Two methods of evaluating the separation efficiency were used; Selectivity Index and Z factor analysis. Tabling and magnetic separation produced poor results, with flotation testing showing some promise, generating concentrates assaying more than 40 per cent Fe. High grade concentrates containing more than 67 per cent Fe were generated using the Kelsey Centrifugal Jig, and it was recommended that this technique be pursued at a larger scale to verify the results obtained.
机译:实验室和飞行员规模测试是在1999年在北美铁矿石厂的尾矿样品中进行的,使用重力,磁性和浮选技术。矿石主要含有16%的铁,主要是在细(-38μm)尺寸分数中。使用了评估分离效率的两种方法;选择性指数和Z因子分析。提取和磁性分离产生了差的结果,浮选测试显示了一些承诺,产生浓缩物测定超过40%的Fe。使用Kelsey离心式夹具产生含有超过67%Fe的高级浓缩物,建议以更大的规模追求该技术以验证所获得的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号