The lead-zinc ore sample containing 3.45 per cent Pb, 3.15 per cent Zn, 12.2g/t Au and 256 g/t Ag was subjected to this experimental study and taken from Bolkarda?-Ni?de, south eastern part of Anatolia. According to the mineralogical studies, the representative ore sample contains primarily native gold, electrum, native silver, and argentojarosite as gold and silver minerals, cerusite, anglesite, galena, pyromorphite, mimetite and plumbojarosite as lead minerals, smithsonite, hydrozincite, hemimorphite, adamite and sphalerite as zinc minerals, limonite, hematite, goethite, pyrite, magnetite and siderite as lead minerals and quartz, feldspar, albite and muscovite as gangue minerals. Beneficiation of complex lead and zinc ore was investigated using flotation method. Various parameters such as particle size, flotation stages, collector type, collector amount, control reagents were investigated to recover of gold and silver bearing minerals. At the end of the experimental studies, the flotation experiments performed with Aero 208+Aerophine 3418 A (350 + 350 g/t) collectors at pH 4.5 gave the best result. -38 microns particle size and 1000 g/t of Na_2SiO_3 as depressant were used at these conditions. At the end of the experiments, a process was designed for evaluation of the ore. According to the process, a concentrate having 920 g/t Au and 10100 g/t Ag can be obtained with the recoveries of 54.1 per cent and 31.1 per cent, respectively.
机译:含有3.45%Pb,3.15%Zn,12.2g / t Au和256g / t Ag的铅锌矿样品进行了该实验研究,并从Bolkarda捕获,从安纳托利亚东部的南部。根据矿物学研究,代表性矿石样品主要含有天然金,电矿,天然银,和argentojarosite,作为金银矿物,Cerusite,Anglesite,Galena,Pyromorphite,Mimetite和Plumbojarosite,如铅矿物,史密松石,羟基胞质,半晶状体,Adamite和硫醇作为锌矿物质,褐铁矿,赤铁矿,甲酸酯,黄铁矿,磁铁矿和赤藓,作为铅矿物和石英,长石,阿尔巴顿和番茄酱作为甘蓝矿物。使用浮选法研究了复合铅和锌矿矿石的矿物。研究了各种参数,例如粒度,浮选阶段,收集器型,收集量,对照试剂,以恢复金和银轴承矿物质。在实验研究结束时,用Aero 208 +荒风3418a(350 + 350g / t)收集器在pH 4.5进行的浮选实验给出了最佳结果。在这些条件下使用-38微米粒径和1000g / t的Na_2siO_3作为抑制剂。在实验结束时,设计了一种用于评估矿石的过程。根据该方法,可以获得920g / t Au和10100g / t Ag的浓缩物,其回收率分别为54.1%和31.1%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号