BIO-OXIDATION OF ARSENIC AND STIBIUM BEARING GOLD ORES

机译:生物氧化砷和体臭金矿

获取原文

摘要

Bio-oxidation of arsenic and stibium bearing gold ores with acidithiobacillus ferrooxidans was studied. The preoxidation results show that the best bio-oxidation technical parameters are the initial pH in the range of 1.8 ~ 2.0, particle sizes under 0.074 mm, temperature in the range of 25 °C ~ 30°C and rotating speed of the orbital incubator in 100 rpm ~ 160 rpm. The leaching results show that If the ore, of which contain 10.37 per cent arsenic and 36.81 per cent stibium, is not bio-oxidised, gold leaching is only about 41 per cent, after 8 days oxidised, the result is about 76.55 per cent, which improved about 35.62 points. The relationship between gold leaching and arsenic oxidation is direct proportion, furthermore, it needs only partly oxidise and higher gold leaching could be get, for example, gold leaching is over 90 per cent when asenic oxidation is 60 per cent. The results will provide theoretical and technological supports of bio-oxidation arsenopyrite for pretreating refractory gold ores.
机译:研究了砷和体臭的生物氧化,含有酸酐铁氧化物的金矿石。预氧化结果表明,最佳的生物氧化技术参数是初始pH值1.8〜2.0,粒度约为0.074 mm,温度范围为25°C〜30°C,轨道孵化器的旋转速度100 rpm〜160 rpm。浸出结果表明,如果矿石,其中含有10.37%的砷和36.81%的体臭,则不是生物氧化,黄金浸出只有约41%,氧化8天后,结果约为76.55%,哪个提高了约35.62点。黄金浸出和砷氧化之间的关系是直接比例,此外,它仅需要部分氧化,并且可以获得更高的金色浸出,例如,当刺激氧化为60%时,金浸出超过90%。结果将提供用于预处理耐火金矿的生物氧化亚苯甲酸盐的理论和技术支持。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号