Corrosion behaviors of Fe_(45-x)Cr_(18)Mo_(14)C_(15)B_6Y_2M_x (M = Al, Co, Ni, N and x = 0, 2) bulk metallic glasses under conditions simulating fuel cell environment

机译:FE_(45-x)CR_(18)的腐蚀行为在条件下模拟燃料电池环境下的散装金属玻璃(M = Al,Co,Ni,N和X = 0,2)散装金属玻璃

获取原文

摘要

The corrosion properties of the Fe_(46-x)Cr_(18)Mo_(14)C_(15)B_6M_x (with M = Al, Co, Ni, N and.x = 0, 2) bulk metallic glasses have been investigated m a 1 M H_2SO_4 + 2 ppm F~- solution at 80 °C with H_2 and air bubbling, which simulate environments of the polymer electrolyte membrane fuel cell. The partial replacement of 2 at.% Fe led to significant modification of the corrosion behavior and resulted in corrosion resistances superior to that of stainless steel.
机译:已经研究了Fe_(46-X)CR_(18)Mo_(14)C_(15)B_6M_X(用M = Al,Co,Ni,N和0,2)散装金属玻璃的腐蚀性。 1 M H_2SO_4 + 2 PPM F〜 - 溶液在80°C的H_2和气鼓中,模拟聚合物电解质膜燃料电池的环境。部分更换为2。%Fe导致耐腐蚀行为的显着改性,导致不锈钢的耐腐蚀性。

著录项

相似文献

  • 外文文献
  • 中文文献
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号