Battery separators are thin, porous membrane of 20-30 microns thickness. Polymer separators display a significant amount of shrinkage at elevated temperatures. It is difficult to quantitatively characterize the large shrinkage behavior with a free standing separator sample. This paper examines the use of a dynamic mechanical analyzer under tensile mode in measuring the coefficient of thermal expansion (CTE) of three commonly used separators.