LOW TEMPERATURE SULPHIDIZATION OF Cu-Co SLAG IN THE PRESENCE OF CALCIUM SULPHIDE

机译:硫化钙存在下Cu-Co渣的低温硫化

获取原文

摘要

The investigation focuses on sulphidization of Cu, Co and Fe from a 7wt%CuO-7wt%CoO-10wt%CaO-40wt% SiO_2-(30 wt%Fe,6 wt%Al)_2O_3 slag in the presence of calcium sulphide (CaS), over a temperature range of 1173 K - 1323 K. The metal oxides phases (CuO, CoO, FeO and Fe_3O_4) in the slag were converted into metal sulphide phases (Cu_2S, CuFeS_2, FeS, Cu_5FeS_4, Co_8S_9) via MO + CaS + SiO_2 = MS + CaSiO_3 reaction, where M represents metallic Cu, Co or Fe. Cu_2S and CoS formed preferentially at low molar ratio of MO/CaS and below 1173 K. The sulphidized slag was reduced in the presence of lime (CaO) and carbon at 1323 K by following the equilibrium: MS + CaO + C = M + CaS + CO(g). The reaction products were characterised by X-ray diffraction and scanning electron microscopy techniques. The proposed method of recovering metallic phases (Cu, Co and Fe) from a Cu-Co slag via sulphidization and reduction at lower reduction temperature than 1373 K offers an energy efficient process.
机译:研究重点是在硫化钙(CaS)存在下,从7wt%CuO-7wt%CoO-10wt%CaO-40wt%SiO_2-((30 wt%Fe,6 wt%Al)_2O_3炉渣中硫化Cu,Co和Fe ),温度范围为1173 K-1323K。通过MO + CaS将炉渣中的金属氧化物相(CuO,CoO,FeO和Fe_3O_4)转化为金属硫化物相(Cu_2S,CuFeS_2,FeS,Cu_5FeS_4,Co_8S_9)。 + SiO_2 = MS + CaSiO_3反应,其中M表示金属Cu,Co或Fe。 Cu_2S和CoS优先在低摩尔比的MO / CaS和低于1173 K的条件下形成。在1323 K的石灰(CaO)和碳存在下,通过遵循以下平衡条件,硫化渣被还原:MS + CaO + C = M + CaS + CO(g)。通过X射线衍射和扫描电子显微镜技术表征反应产物。所提出的通过硫化和在低于1373 K的还原温度下还原进行还原而从Cu-Co炉渣中回收金属相(Cu,Co和Fe)的方法提供了一种节能的方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号