The amount and activity of coal, reduction temperature and other parameters of the process of bottom-blown reduction of liquid high lead slag were investigated in laboratory. Methods to strengthen the bottom-blown reduction process were studied by industrial production. The results were in the follows: the reduction temperature was 1150°C; reduction time was 1.5h; the reductant was anthracite; lead content in slag was controlled to 2%; the rate of coal was 7% and gasification loss of coal in high temperature was severe; liquid lead slag reduction rate was faster with coal; prolonging the reaction size had little effect on reducing lead in slag; the size of the reactor can be further reduced.
机译:研究了实验室研究了煤炭,还原温度和液体高铅渣的底部吹渣的过程的其他参数。通过工业生产研究了加强底部吹制过程的方法。结果如下:还原温度为1150°C;减少时间为1.5h;还原剂是无烟煤;渣中的铅含量控制在2%;煤的速率为7%,高温煤的气化损失严重;煤的液体铅渣还原率更快;延长反应大小对降低渣中的铅几乎没有影响;可以进一步降低反应器的尺寸。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号