Mix proportion design and mechanical property of recycled Polyethylene terephthalate concrete

机译:再生聚对苯二甲酸乙二醇酯混凝土的配合比设计及力学性能

获取原文

摘要

The mix proportion and mechanical property of polyethylene terephthalate (PET) concrete are studied by orthogonal test and mix proportion design. Different limestone, basalt aggregate and mineral is used to mix with melted PET to produce PET concrete. The effect of mineral materials, PET and mineral/aggregate ratio (PETWA/AG), sand ratio, PET/mineral ratio (PET/MA) and materials of coarse aggregate on PET concrete mechanical property is analyzed. The results show that the most important factor is PETWA/AG and then are sand ratio and PET/MA. Basalt is better than limestone as coarse aggregate in PET concrete. From high to low compression strength sequence of PET concrete mixed with different mineral is fly ash with 5% talc, only mixed fly ash or Portland cement (PC), mixed fly ash with 5% asphalt, without any mineral. The best mix proportion of PET concrete is PETWA/AG=1/3, sand ratio=35% and PET/fly ash=2~1.
机译:通过正交试验和配合比设计研究了聚对苯二甲酸乙二醇酯(PET)混凝土的配合比和力学性能。将不同的石灰石,玄武岩骨料和矿物与熔融的PET混合以生产PET混凝土。分析了矿物材料,PET和矿物/骨料比(PETWA / AG),砂比,PET /矿物比(PET / MA)和粗骨料对PET混凝土力学性能的影响。结果表明,最重要的因素是PETWA / AG,然后是砂比和PET / MA。玄武岩比石灰石作为PET混凝土中的粗骨料更好。从高抗压强度到低抗压强度的PET混凝土中,掺有不同矿物的粉煤灰为5%滑石粉,仅掺有掺粉煤灰或硅酸盐水泥(PC),掺有5%沥青的掺粉煤灰,不含任何矿物。 PET混凝土的最佳配合比为PETWA / AG = 1/3,砂比= 35%,PET /粉煤灰= 2〜1。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号