Standardized procedures to measure cleavage fracture toughness of ferritic steels in the DBT region most commonly employ three-point bend fracture specimens, conventionally termed SE(B) or SENB specimens. The evaluation protocol of fracture toughness for these crack configurations builds upon laboratory records of load and crack mouth opening displacement (CMOD) to relate plastic work with J (or, equivalently, CTOD). The experimental approach employs a plastic η-factor to relate the macroscale crack driving force to the area under the load versus crack mouth opening displacement for cracked configurations. This work provides revised η-factors derived from CMOD records applicable to estimate the J-integral and CTOD in SE(B) specimens with varying crack size and specimen configuration. Non-linear finite element analyses for plane-strain and 3-D models provide the evolution of load with increased CMOD which is required for the estimation procedure. The analysis matrix considers SE(B) specimens with W = 2B and W = B configurations with and without side grooves covering a wide range of specimen thickness, including precracked Charpy (PCVN) specimens. Overall, the present results provide further validation of the J and CTOD evaluation procedure currently adopted by ASTM 1820 while, at the same time, giving improved estimation equations for J incorporating 3-D effects which enter directly into more accurate testing protocols for experimental measurements of fracture toughness values using 3P SE(B) specimens.
机译:测量DBT区中铁素体钢的劈裂断裂韧性的标准化程序最常用的是三点弯曲断裂试样,通常称为SE(B)或SENB试样。这些裂纹构型的断裂韧性评估方案建立在载荷和裂纹口张开位移(CMOD)的实验室记录的基础上,以将塑性功与J(或等效地,CTOD)联系起来。实验方法采用塑性η因子将宏观裂纹驱动力与载荷下的面积(裂纹构造的裂纹口张开位移)联系起来。这项工作提供了来自CMOD记录的修正后的η因子,适用于估计具有不同裂纹尺寸和试样构型的SE(B)试样中的J积分和CTOD。平面应变和3-D模型的非线性有限元分析提供了随着CMOD的增加而产生的载荷演化过程,这是估算过程所必需的。分析矩阵考虑具有W = 2B和W = B构型的SE(B)标本,带有和不带有覆盖宽范围试样厚度的侧槽,包括预破裂的夏比(PCVN)标本。总体而言,目前的结果进一步验证了ASTM 1820当前采用的J和CTOD评估程序,同时,给出了结合了3-D效应的J的改进估算公式,这些公式直接输入更准确的测试协议中,用于实验测量使用3P SE(B)试样的断裂韧性值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号