In this experiment,do smell pine impregnated pressure experiments with small molecules phenolic resin.Prepare different small molecules and phenolic resin by orthogonal.Handle the specimens.Compare the treated material with the smell pine.The optimum condition is the temperature of 60°C,PVA:P (mass ratio) =3%,P∶ F∶ NaOH (molar ratio) =1∶1.2∶0.3,the absolute pressure 2.5 Mpa,the temperature of 120 °C hot 15 minutes under the conditions.While smell pine laminated veneer lumber bending strength increased 67.53%.
机译:在本实验中,用小分子酚醛树脂进行松香浸渍压力实验,正交制备不同的小分子和酚醛树脂,处理标本,将处理过的材料与松香进行比较,最佳条件是温度为60°C, PVA:P(质量比)= 3%,P∶F∶NaOH(摩尔比)= 1∶1.2∶0.3,绝对压力2.5 Mpa,在120°C的温度下加热15分钟。单板木材的弯曲强度提高了67.53%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号