A modified bio-polymers was prepared by melt reactive blending Poly(3-hydroxybutyrate-co-4-hydroxybutyrate) [P(3HB-co-4HB)] with commercial chain extenders (ADR-4367). Steady shear and oscillatory measurements were employed to characterize viscoelastic properties of the chain extended bio-polymres. The results show that after P(3HB-co-4HB) is blended with ADR-4367, the co-polymer chains are branched or coupled. Steady shear viscosity of the modified bio-polymers increase by about one order of magnitude, and melts of such polymers behave more viscoelasticity and thermal stability by storage modulus and loss modulus correlated with oscillatory shear frequency and elapsed time. Owing to possessing branches, modified P(3HB-co-4HB) samples have enhanced complex viscosity magnitude and the first normal stress difference values compared with neat P(3HB-co-4HB). Addition of ADR-4367 with contents of 2∼6 wt% brings remarkable effect on improving viscoelastic properties of the modified bio-polymers.
机译:通过将聚(3-羟基丁酸酯-co-4-羟基丁酸酯)[P(3HB-co-4HB)]与商用扩链剂(ADR-4367)熔融反应共混来制备改性的生物聚合物。使用稳态剪切和振荡测量来表征扩链生物聚合物的粘弹性质。结果表明,将P(3HB-co-4HB)与ADR-4367共混后,共聚物链分支或偶联。改性生物聚合物的稳态剪切粘度增加约一个数量级,并且这种聚合物的熔体通过与振荡剪切频率和经过时间相关的储能模量和损耗模量表现出更大的粘弹性和热稳定性。由于具有分支,与纯净的P(3HB-co-4HB)相比,改性的P(3HB-co-4HB)样品具有更高的复数粘度幅度和第一个法向应力差值。加入2〜6wt%的ADR-4367对改善改性生物聚合物的粘弹性具有显着的效果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号