UNDERPROTECTION OF MILD STEEL IN SEAWATER AND THE ROLE OF THE CALCAREOUS FILM

机译:海水中钢水的保护不足和钙化膜的作用

获取原文

摘要

Under normal conditions cathodically protected mild steel in seawater is also protected by a precipitated film of calcium carbonate and magnesium hydroxide, the so-called calcareous film. Under certain circumstances, underprotection can occur, for example; where current demand values are under estimated, or where structures are approaching the end of their design lives and anodes are severely reduced in size, or at cold deep water situations where the calcareous film is more soluble and reluctant to form. In these situations, a calcareous film might well occur but complete protection is probably not possible. These conditions are being studied in the laboratory using artificial seawater and protection current densities less than would be normally applied in practice. Experiments involving weight loss, ac impedance and surface analysis will be described to attempt to clarify the situation under these interesting conditions.
机译:在正常情况下,海水中的阴极保护的温和钢也受到碳酸钙和氢氧化镁的沉淀薄膜的保护,所谓的钙质薄膜。例如,在某些情况下,可能会发生欠款;在估计当前需求值的情况下,或者在其设计中的结构终止的情况下,阳极尺寸严重减小,或者在钙质薄膜更溶于和不愿表的情况下严重降低。在这些情况下,钙质电影可能很好地发生,但可能无法完全保护。使用人造海水在实验室中研究了这些条件,并且保护电流密度小于通常在实践中的应用。将描述涉及体重减轻,交流阻抗和表面分析的实验,以澄清这些有趣条件下的情况。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号