Mixing behaviors of the compounds filled with different reinforcing fillers were studied in correlation with compound and vulcanizate properties. Four filler systems were used including: 1) silica plus small amount of silane coupling agent; 2) carbon black; 3) pre-modified silica; and 4) silica+silane-carbon black mixed one. The results have shown that silica provides longer optimum cure time and shorter cure rate than carbon black due to accelerator adsorption on silica surface. In addition, owing to highly polar nature on silica surface the silica-based compounds show rather high viscosity, attributed to stronger filler-filler interaction as can be confirmed by Payne effect and reinforcement index. However, the commercial surface treatment or pre-modified form of silica shows superior properties than in-situ modification of silica by silane during mixing, while it gives comparable properties to carbon black-based compound. Tensile properties of vulcanizates show a good correlation with the basic properties of their compounds.
机译:研究了填充有不同增强填料的胶料的混合行为,并与胶料和硫化胶的性能相关。使用了四种填料体系,包括:1)二氧化硅加少量硅烷偶联剂; 2)炭黑; 3)预改性的二氧化硅; 4)二氧化硅+硅烷-炭黑混合之一。结果表明,由于促进剂吸附在二氧化硅表面上,与炭黑相比,二氧化硅提供了更长的最佳固化时间和更短的固化速率。另外,由于二氧化硅表面上的高极性性质,基于二氧化硅的化合物显示出相当高的粘度,这归因于更强的填料-填料相互作用,这可以通过佩恩效应和增强指数得到证实。然而,商业化的表面处理或二氧化硅的预改性形式显示出比在混合过程中通过硅烷原位改性二氧化硅更好的性能,同时它提供了与基于炭黑的化合物相当的性能。硫化橡胶的拉伸性能与其化合物的基本性能显示出良好的相关性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号