首页> 外文会议>International conference on nuclear engineering >CORROSION IN STEEL T91 CAUSED BY FLOWING LEAD-BISMUTH EUTECTIC AT 400 °C AND 10~(-7) MASS SOLVED OXYGEN
【24h】

CORROSION IN STEEL T91 CAUSED BY FLOWING LEAD-BISMUTH EUTECTIC AT 400 °C AND 10~(-7) MASS SOLVED OXYGEN

机译:通过在400℃和10〜(-7)质量%溶解的氧气下流动的铅 - 铋引起的钢T91引起的腐蚀引起的

获取原文

摘要

Specimens produced from two different heats of ferritic/martensitic steel T91 were exposed to oxygen-containing flowing lead-bismuth eutectic (LBE) at 400 °C, 10~7 mass% solved oxygen and flow velocity of 2 m/s, for exposure times between around 1000 and 13,000 h. The occurring phenomena were analyzed and quantified using metallographic cross sections prepared after exposure. Oxidation causes a material loss of <10 μm after 13,000 h, while corrosion initiated by the solution of the steel elements may generally proceed around 15 to 30 μm deep into the material in the same amount of time. Oxide scales formed on both heats of T91 tend to buckle and detach. In the case of one of the investigated heats, a singular event of exceptionally severe solution-based corrosion was observed, with associated local material loss around 1.2 mm after 13,000 h. The results are compared especially with findings at 450 and 550 °C and otherwise similar conditions as well as austenitic steels tested in the identical experimental run.
机译:由两种不同的铁素体/马氏体钢T91产生的样品暴露于含氧流动的流动的引入铋共晶(LBE),在400℃下,10〜7质量%溶解的氧气和2m / s的流速,用于暴露时间大约1000和13,000小时之间。使用暴露后制备的金相横截面分析和量化发生的现象。氧化导致13,000小时后的材料损失<10μm,而通过钢元件的溶液引发的腐蚀通常可以在相同的时间内深入地进入材料中的约15至30μm。在T91的两个热量上形成的氧化物鳞倾向于弯曲和分离。在其中一种研究的热量的情况下,观察到非苛性溶液的溶液的奇异事件,在13,000小时后,相关的局部材料损失约为1.2mm。比较结果,特别是在450和550°C的结果,以及其他类似的条件以及在相同的实验运行中测试的奥氏体钢。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号