Current estimates and glass formulation efforts are conservative vis-a-vis achievable waste loadings. These formulations have been specified to ensure that glasses are homogenous, contain essentially no crystalline phases, are processable in joule-heated, ceramic-lined melters and meet WTP Contract terms. The WTP's overall mission will require the immobilization of tank waste compositions that are dominated by mixtures of aluminum, chromium, bismuth, iron, phosphorous, zirconium, and sulfur compounds as waste-limiting components. Glass compositions for these waste mixtures have been developed based upon previous experience and current glass property models. DOE has a testing program to develop and characterize HLW glasses with higher waste loadings. This work has demonstrated the feasibility of increases in waste loading from 25 wt% to 33-50 wt% (based on oxide loading) in the glass depending on the waste stream. It is expected these higher waste loading glasses will reduce the HLW canister production requirement by 25% or more.
机译:当前的估计和玻璃配方的努力相对于可实现的废物负荷而言是保守的。已指定这些配方,以确保玻璃均匀,基本不含晶相,可在焦耳加热的陶瓷衬里熔炉中加工并符合WTP合同条款。 WTP的总体任务将需要固定以铝,铬,铋,铁,磷,锆和硫化合物作为限制废物成分的混合物为主的储罐废物成分。基于先前的经验和当前的玻璃性能模型,已经开发出用于这些废物混合物的玻璃组合物。美国能源部有一项测试计划,以开发和鉴定具有更高废物负荷的高放废物玻璃。这项工作已经证明了根据废物流将玻璃中的废物负载量从25 wt%增加到33-50 wt%(基于氧化物负载量)的可行性。预计这些较高的废料装载玻璃将使HLW罐的生产需求减少25%或更多。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号