Modification of (y)-Al2O3 as Ink-Jet Printing Paper Coating Pigment by Coupling Agents

机译:偶联剂对(y)-Al2O3喷墨印刷纸涂料颜料的改性

获取原文

摘要

γ-Al2O3 namely activated alumina or alumina gel is widely used as a pigment on the inkjet paper at present.But it is easy to come out a particles agglomeration problem to restrict its application.In this paper,the γ-Al2O3 with coupling agents were modified to improve its dispersion in water.In the modification process,the he main modification parameters such as aluminum-zirconium complex oligomeric coupling agent TL-3A were selected to study.The parameters of addition,modification time and modification temperature were discussed.During the experiment,the best modification conditions were determined via orthogonal experiments.The polydispersity index PDI was used the target parameters to inspect via orthogonal experiments results and the affected factors.We found the best addition quantity of coupling agent,modification time and modification temperature to reach the minimum of the polydispersity index PDI introduction.The results showed that the best condition for carbonization alumina was:the best condition for export γ-Al2O3 2.0%,modification time 30min,modification temperature 50°C.
机译:γ-Al2O3(即活性氧化铝或氧化铝凝胶)目前在喷墨纸上被广泛用作颜料,但很容易出现颗粒团聚的问题,限制了其应用。在改性过程中,主要研究了铝锆复合低聚物偶联剂TL-3A等主要改性参数,研究了添加,改性时间和改性温度等参数。正交实验确定了最佳的修饰条件。以多元分散指数PDI为目标参数,通过正交试验结果和影响因素,确定了偶联剂的最佳添加量,修饰时间和修饰温度达到了最佳。结果表明,最佳的碳化条件是氧化铝。最佳条件为:γ-Al2O3的最佳出料率为2.0%,改性时间为30min,改性温度为50℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号