The simultaneous desulphurization and dephosphorization of molten steel with CaO-based slag containing BaO for vacuum treatment,and inclusion in steel and microstructure of steel are carried out separately.These results show that desulfurization rate exceed 92% and dephosphorization rate exceed 50%,final [S] content and [P] content in molten steel are less than 0.0024% and 0.020% respectively for all heats,and the lowest final [S] content and [P] content are 0.0012% and 0.010% respectively,they satisfy the demand of ultra-low S steels and low P steels;Comparing a grade 1.5 of inclusion level of the compared sample without vacuum treatment,inclusion level of these treated samples with vacuum is all less than grade 1.0 and that is less than grade 0.5 for 78% of treated samples; And micro-structure of the compared sample is ferrite + pearlite in steel base,but micro-structure of these treated samples is all needle-like fenrite + pearlite + netted ferrite in steel base and netted ferrite + pearlite in local area.This kind of fiber structure which comes from netted ferfite + needle-like ferrite and grade 0.5 of inclusion level can make steel possess better mechanical properties.
机译:用含BaO的CaO基炉渣对钢水同时进行脱硫和脱磷,并同时进行钢中的夹杂物和钢的微观结构。结果表明,脱硫率超过92%,脱磷率超过50%,最终[所有钢水中钢中的S]含量和[P]含量均小于0.0024%和0.020%,最低的最终[S]含量和[P]含量分别为0.0012%和0.010%,它们满足以下要求:超低硫钢和低磷钢;与未进行真空处理的比较样品的夹杂物等级为1.5级相比,这些经过真空处理的样品的夹杂物含量均低于1.0级,而对于78%的样品,夹杂物含量低于0.5级。处理过的样品;比较样品的显微组织是钢基中的铁素体+珠光体,但这些处理过的样品的显微结构都是钢状的针状fenite +珠光体+网状铁素体,局部是网状铁素体+珠光体。网状铁素体+针状铁素体形成的纤维结构,夹杂物含量为0.5级,可使钢具有更好的力学性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号