To look into the ionic release laws of the sulphide tailings in some copper mine, the effects of the soaking period, temperature, oscillating speed, and pH of the solution on the heavy metals ionic release were investigated through static soaking leaching experiments. The results show that Cu2+,Zn2+, Pb2+, Cr3+ are of different leaching behaviors with soaking period. The ionic concentration in soaking solution for four ions has a great gap. Zn2+ is more easily released out of sulfide tailings than Cuz+, Pb2+, Cr3+, and the ion release concentrations are not proportion to their contents in the tailings. The time for each ion to reach its maximum concentration are different. The minimum concentration do not occur at the first day. Each ion concentration shows different fluctuation characteristic during soaking process. Solution pH, oscillating speed, and temperature affect the releases of Cu2+, Zn2+, Pb2+, Cr3+ out of the tailings to different extent. The effect of pH value on ion release for the four ions ranks as Zn2+>Cu2+>pb2+>Cr3+, the oscillating speed ranks as Pb2+>Zn2+>Cu2+>Cr3+, and the temperature ranks as Cr3+>Pb2+>Zn2+>Cu2+.
机译:为了研究某铜矿中硫化物尾矿的离子释放规律,通过静态浸泡浸出实验研究了浸泡时间,温度,振荡速度和pH值对重金属离子释放的影响。结果表明,Cu 2+,Zn 2+,Pb 2+,Cr 3+随浸泡时间的不同而有不同的浸出行为。浸泡液中的四个离子的离子浓度之间存在较大的差距。 Zn2 +比Cuz +,Pb2 +,Cr3 +更容易从硫化物尾矿中释放出来,并且离子释放浓度与尾矿中的含量不成比例。每个离子达到其最大浓度的时间是不同的。最低浓度不会在第一天出现。在浸泡过程中,每种离子浓度都表现出不同的波动特性。溶液的pH值,振荡速度和温度对尾矿中Cu2 +,Zn2 +,Pb2 +,Cr3 +的释放有不同程度的影响。 pH值对4种离子的离子释放的影响依次为Zn2 +> Cu2 +> pb2 +> Cr3 +,振荡速度为Pb2 +> Zn2 +> Cu2 +> Cr3 +,温度为Cr3 +> Pb2 +> Zn2 +> Cu2 +。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号