The flotation circuit and the reagents of the all-sliming flotation about low grade and hard operation on zinc oxide ore are researched in the paper.The results indicated that there are many types of zinc minerals in this ore, and the composition is very complex. They include hemimorphite, smithsonite, hydrozincite and so on. The ore is seriously sliming. In light of the ore properties, three kinds of flowsheets have tested. They are gravity concentration (cleaning tables), flotation, combined process of gravity concentration and flotation.The test showed that the recovery of zinc is only 17.08% in the gravity separation. In combined process of gravity separation and flotation, the recovery of zinc concentrate is close to 70%. But the flow-sheet is complex and hard to control in the production. The floatation circuit is feasible. In the test, it pay attention to investigate the new combined reagent which is used in selective all-sliming flotation process. The effects of slime are eliminated by the multi-loop treatment of middling. In flotation, the final recovery of concentrate is 88.76%; the grade is 29.50%. The recovery of physical ore is 93%; and the recovery of -10mm fraction is more than 65%.
机译:研究了氧化锌矿的低品位,难操作的全矿浮选工艺及全浆浮选试剂,结果表明该矿中锌矿物种类繁多,组成非常复杂。它们包括半晶石,史密斯石,水锌矿等。矿石严重变稀。根据矿石性质,已经测试了三种流程图。它们是重力浓缩(清洁台),浮选,重力浓缩和浮选的组合过程。试验表明,重力分离中锌的回收率仅为17.08%。在重力分离和浮选的组合过程中,锌精矿的回收率接近70%。但是流程图很复杂,在生产中很难控制。浮动电路是可行的。在试验中,要注意研究选择性全浮选浮选过程中使用的新型混合试剂。粘液的污垢通过中环的多回路处理而消除。在浮选中,精矿的最终回收率为88.76%;等级是29.50%。物理矿石的回收率为93%; -10mm分数的回收率超过65%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号