Um-Gheig Pb-Zn representative sample was collected from the main adite of Um-Gheig mine along Red Sea coast in Egypt. Its chemical analysis shows that, it contains 16% Zn, 2.3% Pb, 0.1% Cd and 0.1% B as elements of interest. After H2SO4 agitation leaching, the chemical composition of Um-Gheig Pb-Zn deposit ore residue assayed 2.26% Pb, 1.5% Zn, 0.085 % B and 0.01% Cd. This residue was leached with 20% HC1 at S/L ratio 1/3 for 2 hours at 80°C. The chloride leach liquor was found to contain 18 g/l Pb, 13 g/l Zn, 0.1 g/l Cd and 0.75 g/l B with the corresponding leaching efficiencies 79%, 86%, 100% and 88% respectively.Lead was precipitated from the chloride leach liquor using concentrated H_2SO_4 to obtain PbSO_4 with precipitation efficiency 96%. While boron was extracted by the selective resin Amberlite IRA743 with loading efficiency of 80%. On the other hand, Zn and Cd were precipitated using solution with 86.7% and 100% recovery efficiencies respectively.
机译:Um-Gheig Pb-Zn代表性样品是从埃及红海沿岸的Um-Gheig矿的主要矿床采集的。其化学分析表明,它含有16%的Zn,2.3%的Pb,0.1%的Cd和0.1%的B作为目标元素。 H2SO4搅拌浸出后,Um-Gheig Pb-Zn矿床矿石残留物的化学成分为2.26%Pb,1.5%Zn,0.085%B和0.01%Cd。该残余物在80℃下以20%的S / L比率用20%的HCl浸提2小时。发现氯化物浸出液含有18 g / l的Pb,13 g / l的Zn,0.1 g / l的Cd和0.75 g / l的B,相应的浸出效率分别为79%,86%,100%和88%。 使用浓H_2SO_4从氯化物浸出液中沉淀出铅,得到PbSO_4,沉淀效率为96%。硼是由选择性树脂Amberlite IRA743提取的,负载效率为80%。另一方面,使用回收率分别为86.7%和100%的溶液沉淀Zn和Cd。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号